Sign In | Join Free | My infospaceinc.com |
|
Brand Name : OHMALLOY
Model Number : cuni constantan
Certification : ISO9001-2008
Place of Origin : China(Shanghai)
MOQ : 20KG
Price : 20-50USD/KG
Payment Terms : L/C, T/T, , MoneyGram
Supply Ability : 50 Tons per month
Delivery Time : 7-10 days
Packaging Details : Roll/Spool
Material : constantan
Density (g/cm3) : 8.9
Electrical resistivity at 20℃ (Ωmm2/m) : 0.49
Tensile Strength : 420Mpa
Yield strength : 250Mpa
Elongation : 25%
Constantan( Ohmalloy 049)
(Common Name: CuNi45, NC50.Cuprothal, Alloy 294, Cuprothal 294, Nico, MWS-294, Cupron, Copel, Alloy 45, Neutrology, Advance, CuNi 102, Cu-Ni 44, Konstantan,constantan.)
OhmAlloy049 is a copper-nickel alloy (Cu56Ni44 alloy) characterized by high electrical resistance, high ductility and good corrosion resistance. It is suitable for use at temperatures up to 400°C
Typical applications for OhmAlloy49 are temperature-stable potentiometers, industrial rheostats and electric motor starter resistances.
The combination of negligible temperature coefficient and high resistivity makes the alloy particulary suitable for the winding of precision resistors.
OhmAlloy049 is manufactured from electrolytic copper and pure nickel. In finer wire sizes the alloy is designated as OhmAlloy49TC(Thermocouple).
Nickel | 45 | Manganese | 1 |
Copper | Bal. |
Yield strength | Tensile Strength | Elongation |
Mpa | Mpa | % |
250 | 420 | 25 |
Density (g/cm3) | 8.9 |
Electrical resistivity at 20℃ (Ωmm2/m) | 0.49 |
Temperature factor of resistivity(20℃~600℃)X10-5/℃ | -6 |
Conductivity coefficient at 20℃ (WmK) | 23 |
EMF vs Cu(μV/℃ )(0~100℃ ) | -43 |
Coefficient of thermal expansion |
|
Temperature | Thermal Expansion x10-6/K |
20 ℃- 400℃ | 15 |
Specific heat capacity | |
Temperature | 20℃ |
J/gK | 0.41 |
Melting point (℃) | 1280 |
Max continuous operating temperature in air (℃) | 400 |
Magnetic properties | non-magnetic |
Corrosion resistance performance
Alloys |
Working In atmosphere at 20℃ |
Working at max temperature 200℃ | ||||
Air and oxygen contain gases |
gases with Nitrogen |
gases with sulfur oxidability |
gases with sulfur reductibility |
carburization | ||
OhmAlloy049 | good | good | good | good | bad | good |
Style of supply
Alloys Name | Type | Dimension | |
OhmAlloy049W | Wire | D=0.03mm~8mm | |
OhmAlloy049R | Ribbon | W=0.4~40 | T=0.03~2.9mm |
OhmAlloy049S | Strip | W=8~200mm | T=0.1~3.0 |
OhmAlloy049F | Foil | W=6~120mm | T=0.003~0.1 |
OhmAlloy049B | Bar | Dia=8~100mm | L=50~1000 |
![]() |
Winding Heating Resistance Wire Constantan / Copper Nickel / CuNi44 Material Images |